THE PARAMETERS AFFECTING ADHESION OF HDG COATING

1 KREISLOVA Katerina
Co-authors:
1 GEIPLOVA Hana 1 TUREK Libor 1 BARTAK Zdenek 2 KUDLACEK Jan
Institutions:
1 SVUOM Ltd., Prague, Czech Republic, EU
2 CVUT, Faculty of Machinery, Prague, Czech Republic, EU
Conference:
25th Anniversary International Conference on Metallurgy and Materials, Hotel Voronez I, Brno, Czech Republic, EU, May 25th - 27th 2016
Proceedings:
Proceedings 25th Anniversary International Conference on Metallurgy and Materials
Pages:
904-909
ISBN:
978-80-87294-67-3
ISSN:
2694-9296
Published:
14th December 2016
Proceedings of the conference were published in Web of Science and Scopus.
Metrics:
343 views / 771 downloads
Abstract

The paper shows the evaluation of delamination of HDG coating. The HDG coating adhesion was evaluated by impact test and by pull-off test. The effect of substrate steel chemical composition, metallurgical conditions and other parameters influencing the quality of zinc coating, mainly the intermetallic phases, are described. The silicon content in aluminium-killed steel was identified as crucial factor for tested samples. The result of adhesion test corresponds to structure of zinc coating.

Keywords: HDG coating, adhesion, steel chemical composition, intermetallic phases