POSSIBILITES OF THE CONTROLLED GASIFICATION OF ALUMINUM ALLOYS FOR ELIMINATING THE CASTING DEFECTS

1 LICHÝ Petr
Co-authors:
1 KROUPOVÁ Ivana 1 RADKOVSKÝ Filip 1 NGUYENOVÁ Isabel
Institution:
1 VSB - Technical University of Ostrava, Ostrava, Czech Republic, EU, petr.lichy@vsb.cz
Conference:
25th Anniversary International Conference on Metallurgy and Materials, Hotel Voronez I, Brno, Czech Republic, EU, May 25th - 27th 2016
Proceedings:
Proceedings 25th Anniversary International Conference on Metallurgy and Materials
Pages:
1474-1479
ISBN:
978-80-87294-67-3
ISSN:
2694-9296
Published:
14th December 2016
Proceedings of the conference were published in Web of Science and Scopus.
Licence:
CC BY 4.0
Metrics:
1424 views / 851 downloads
Abstract

The work deals with the controlled gasification of castings from aluminum alloys. In troubled places of castings the thermal nodes that cannot be always fitted with risers and interior shrinkage with negative influence on tightness and the mechanical properties of casting are formed. If a riser cannot be used for eliminating the negative impact then it is possible to use the Probat Fluss Mikro 100 product. The practical part of the work deals with the monitoring of controlled gasification which creates as a result of adding the Probat Fluss Mikro 100 product and titanium hydride in various proportions. Using the Probat Fluss Mikro 100 as nucleating phase and then with the aid of titanium hydride the hydrogen are brought in the melt. With the aid of visual comparison the effect of controlled gasification is evaluated.

Keywords: Aluminum alloys, gases in the metal, hydrogen, titanium hydride, volume changes

© This is an open access article distributed under the Creative Commons Attribution License which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.